LEXAN™ 201R resin
Polycarbonate
SABIC Innovative Plastics
产品说明:
7.0 MFR, for thicker sections without sinks. Improved flame retardance. Internal mold release.
物性信息:
黄卡编号 |
|
特性 |
|
加工方法 |
|
比重 | ASTM D792 | ||
-- | 1.20 | g/cm³ | ASTM D792 |
-- | 1.19 | g/cm³ | ASTM D792 |
特定体积 | 0.835 | cm³/g | ASTM D792 |
熔流率(熔体流动速率)(300°C/1.2 kg) | 7.0 | g/10 min | ASTM D1238 |
收缩率 - 流动(3.20 mm) | 0.50 到 0.70 | % | 内部方法 |
吸水率 | ASTM D570 | ||
24 hr | 0.15 | % | ASTM D570 |
平衡, 23°C | 0.35 | % | ASTM D570 |
平衡, 100°C | 0.58 | % | ASTM D570 |
室外适用性 | f2 | UL 746C |
洛氏硬度 | ASTM D785 | ||
M 级 | 70 | ASTM D785 | |
R 级 | 118 | ASTM D785 |
抗张强度1 | ASTM D638 | ||
屈服 | 62.1 | MPa | ASTM D638 |
断裂 | 68.9 | MPa | ASTM D638 |
伸长率2 | ASTM D638 | ||
屈服 | 7.0 | % | ASTM D638 |
断裂 | 140 | % | ASTM D638 |
弯曲模量3(50.0 mm 跨距) | 2340 | MPa | ASTM D790 |
弯曲强度4(屈服, 50.0 mm 跨距) | 97.9 | MPa | ASTM D790 |
泰伯耐磨性(1000 Cycles, 1000 g, CS-17 转轮) | 10.0 | mg | ASTM D1044 |
悬壁梁缺口冲击强度(23°C) | 910 | J/m | ASTM D256 |
无缺口悬臂梁冲击(23°C) | 3200 | J/m | ASTM D4812 |
装有测量仪表的落镖冲击(23°C, Energy at Peak Load) | 65.0 | J | ASTM D3763 |
落锤冲击(23°C) | 169 | J | ASTM D3029 |
拉伸冲击强度5 | 630 | kJ/m² | ASTM D1822 |
载荷下热变形温度 | ASTM D648 | ||
0.45 MPa, 未退火, 6.40 mm | 138 | °C | ASTM D648 |
1.8 MPa, 未退火, 6.40 mm | 132 | °C | ASTM D648 |
维卡软化温度 | 154 | °C | ASTM D15256 |
线形热膨胀系数 - 流动(-40 到 95°C) | 6.8E-5 | cm/cm/°C | ASTM E831 |
比热 | 1260 | J/kg/°C | ASTM C351 |
导热系数 | 0.29 | W/m/K | ASTM C177 |
RTI Elec | 130 | °C | UL 746 |
RTI Imp | 130 | °C | UL 746 |
RTI | 130 | °C | UL 746 |